Microstructure and conductivity evolution in Bi2CuO4–Bi2O3 and Bi2MoO6–Bi2Mo2O9 oxide composites nearby eutectic temperatures

N. V. Lyskova, Yu. G. Metlinb, D. V. Vinogradovab, Yu. D. Tret'yakovb

a Department of Materials Science, M.V. Lomonosov Moscow State University, Moscow, Russian Federation
b Department of Chemistry, M.V. Lomonosov Moscow State University, Moscow, Russian Federation

Аннотация: The enhance of electrical conductivity at the eutectic temperature was attended with a thermally reversible microstructural change of composites, expressed by redistribution of an eutectic liquid between triple grain junctions (at cooling) and grain boundaries (at heating).