Specific features of synthesis of detonation nanodiamonds

V. V. Danilenko

ALIT Joint-Stock Company, Kiev, 03067, Ukraine

Abstract: It is demonstrated that the Chapman–Jouguet parameters for high explosives used in nanodiamond synthesis are located in the region of liquid nanocarbon; therefore, the chemical reaction zone of the detonation wave involves formation of carbon nanodroplets, which are later crystallized into nanodiamonds on the segment of the isentrope of expansion of detonation products, passing through the region of stability of nanodiamonds in the pressure range of 16.5–10 GPa and the temperature range of 3400–2900 K. Soot in the resultant mixture is the product of amorphization of nanodroplets rather than graphitization of ultrafine diamonds. The influence of detonation conditions of high-explosive charges in an explosive chamber on nanodiamond synthesis is analyzed.

Keywords: nanodiamond, synthesis, amorphization, detonation, scale factor.

UDC: 534.222.2:553.81

Received: 16.11.2004


 English version:
Combustion, Explosion and Shock Waves, 2005, 41:5, 577–588